Figure 7
(a) The strain dependence of the d spacing and intensity of the diffractions appearing on the meridian in the edge pattern. The diffractions are indexed to 001 and [0 0 {\overline 1}] of the primitive lattice in the region of strain below 35%. (b) The corresponding stress–strain curve (SS-curve) of the SPNP film during uniaxial stretching at 10% min−1.