Figure 2
Temperature dependence of the longitudinal resistivity for (o-Me2TTF)2NO3. The red solid (dashed) curve is the fit to the high-temperature (low-temperature) data with ρ = ρ0 exp(Eact/T). The higher resistivity observed in the warming cycle is attributed to cracks affecting the crystal during the initial cooling process. |