Previous studies for P4W16O56: XRD pattern obtained by Ottolenghi et al. (1995BB25) at 37 K and resistivity measurements published by Dumas et al. (2000BB5). Changes have been applied to the original figure; red circles show the positions of the main reflections and some satellite reflections and axes are highlighted with more contrast.