view article

Figure 1
Starting material and target assemblage of the shock-recovery experiments. (a), (b) The target assemblies of shots 1253 and 1255, respectively. Two wedges cut from one Al–Cu–W GDI disk were used for the two experiments. The size of the SS304 chamber and Ta/steel impactor plate are schematic and are not proportional to the sample size. (c), (d) SEM BSE image of the cross section of the starting GDI. The Al–Cu gradient is shown in the middle of (c). A high-magnification image of the transitional part is shown in (d).

IUCrJ
Volume 7| Part 3| May 2020| Pages 434-444
ISSN: 2052-2525