view article

Figure 2
The overall image of the shocked GDI wedge of S1253 and its deformed zones. (a), (b) represent reflected light and BSE images of the sample. The ramp of the wedge is deformed into an L shape and reaction is concentrated along the right wall. (c) A BSE image of the boxed area in (b). Reactions between the GDI and the steel chamber occur along the right and left edges of the GDI material, which began before deformation as the Al top and Al–Cu ramp of the GDI, respectively. The boxed area is shown in Fig. 3[link].

IUCrJ
Volume 7| Part 3| May 2020| Pages 434-444
ISSN: 2052-2525