view article

Figure 3
(a) An illustration of the perpendicular measurement geometry of the 2D WAXD experiments. The 2D WAXD patterns of (b) P4MP1 bulk and the (c) 30, (d) 50, (e) 70 and (f) 300 nm rods. The nanorods within the template were crystallized isothermally at Tx = 100 °C for about 8 h before the WAXD experiments.

IUCrJ
Volume 8| Part 2| March 2021| Pages 215-224
ISSN: 2052-2525