Figure 3
Simulation of the Vitroperm SANS contrast signal as a function of the sample thickness, with and without depolarization. For the comparison, the parameters determined by the transmission depolarization measurement at 17 mT are taken: μ = 0.032 sheet−1 and D = 0.016 sheet−1. Considering the depolarization, the optimum thickness shifts from 1/μ = 31.3 to 25.3 sheets.

IUCrJ
Volume 8| Part 3| May 2021| Pages 455-461