disable zoom     view article     reuse permissions

Figure 2
(a) Morphological change during heating. The recover processes of spherulites at 135°C after melting at (b) 170, (c) 172 or (d) 174°C. To see the crystal grains in (c) clearly, colored images were changed to gray images.