view article

Figure 2
(a)–(c) Crystals of form III, IV and II, respectively, found in a sample after crystallization for 30 s on a TEM grid. Scale bars = 2 µm. The insets show representative frames from the data collections. (d)–(f) Corresponding 3D ED reciprocal lattice reconstructions all viewed along b*. All images were measured at 100 K.