Figure 1
GPA of the SEM micrograph. (a) Typical SEM micrograph of the prepared Au colloidal crystals. Two ROIs are selected and indicated by the yellow-dashed lines. (b) and (d) Simulated diffractions of ROI I and ROI II. (c) and (e) Fourier transform of the diffraction peak S1 and S2 marked by red boxes in (b) and (d), respectively.