view article

Figure 4
(Top row) A 5 µm ESRF logo test sample imaged by (left) SEM, (middle) CXDI before the EBS at 32.5 nm pixel size and (right) with the EBS at 7.6 nm pixel size. (Bottom row) Enlargements of the letter `R' demonstrate the increase in resolution.

IUCrJ
Volume 12| Part 3| May 2025| Pages 280-287
ISSN: 2052-2525