Thermal expansion of (Sr1−x, K2x)Zr4(PO4)6 (SrKZP) (with x = 0–1) ceramic was investigated using both a dilatometer and a high-temperature X-ray diffractometer. The coefficients of thermal expansion (CTEs) of the SrKZP ceramic measured by the dilatometer demonstrate a similar trend as those from high-temperature X-ray diffraction. Both measurements show an ultra-low CTE at x = 0.5; nevertheless, this composition shows significant lattice thermal-expansion anisotropy (TEA), while the minimum TEA appears with composition x = 0.2. Although it possessed a sufficient degree of TEA, the x = 0.5 composition showed no visible microcracks or negligible microcracks over a grain size as large as 15 μm. A transition of space group from R{\bar 3} to R{\bar 3}c with composition between x = 0.3 and x = 0.5 has been observed. The crystal structure of the SrKZP ceramic with possible occupations of strontium and/or potassium within the lattice in relation to their influence on the CTEs is proposed.
Follow J. Appl. Cryst.
Sign up for e-alerts
Follow J. Appl. Cryst. on Twitter
Follow us on facebook
Sign up for RSS feeds