Figure 2
A comparison of the experimental glancing-angle dependence of the CEY signal for the 1300 (solid line) and 200 Å (dashed line) Au films, and the calculated glancing-angle dependence of the X-ray penetration depth (open circles). |
|
Figure 2
A comparison of the experimental glancing-angle dependence of the CEY signal for the 1300 (solid line) and 200 Å (dashed line) Au films, and the calculated glancing-angle dependence of the X-ray penetration depth (open circles). |