view article

Figure 1
Energy-dispersive pattern collected from the uranium-containing glass using a polychromatic beam of X-rays to stimulate the fluorescence. The Pulser peak was added electronically as an aid to checking the stability of the detector electronics. The unassigned peaks at low energy are due to escape events (Stuan Olsen, 1974BB7).