Plot of d spacing versus strain for an experiment where a single strut of PU foam was incrementally strained to ∼2.1. There was a loss in diffracted SAXS intensity above a strain of ∼1.5 which is attributed either to the sample moving relative to the X-ray beam or to a loss of long-range structural order.