Figure 2
Electron yield spectra of a thick 20 ML Co film at 17° grazing X-ray incidence. The data were collected using BL 5.2 and the EPU (see text). The strong dichroic signal results from the high film quality and the high degree of circular polarization of the EPU, of 0.95 (5). The data were collected at 300 K. |