Figure 2
(a) TRXRD patterns recorded in the FZ of the manganese–carbon steel weld at a position 3 mm from the weld center. The parameters are 12 keV, 730 µm pinhole and 50 ms time resolution. For clarity, only every 15th of the 600 frames is plotted. (b) A temperature–time schematic depicting the recorded TRXRD events given in (a). The scale for the temperature axis is discussed in the text. |