Figure 6
A comparison of the diffraction pattern of polypropylene collected at the ESRF (black curve) and on station 6.2 at Daresbury (red curve). The MPW6.2 data have higher angular resolution and higher integrated peak intensities. The gas–glass microstrip detector used at the ESRF does not suffer from the over-channel anomalies of RAPID2 and currently gives a smoother background. |