Figure 10
Pt foil (light line) and reduced 1%Pt–15%Co/Al2O3 catalyst (dark line) k3-weighted χ(k) spectra. Catalyst reduced at 673 K in situ with hydrogen and cooled under hydrogen. |
|
Figure 10
Pt foil (light line) and reduced 1%Pt–15%Co/Al2O3 catalyst (dark line) k3-weighted χ(k) spectra. Catalyst reduced at 673 K in situ with hydrogen and cooled under hydrogen. |