Figure 1
(a) Structure for the FePd alloy in the L10 phase leading to perpendicular magnetic anisotropy (i.e. normal to the layers). (b) Magnetic force microscopy image measured from the top layer of a 40 nm FePd thin film displaying magnetic stripes, where the perpendicular magnetization component alternates between pointing up and down. |