Figure 7
The Ce M4,5-edge XANES from 40 wt% graphite and 60 wt% of 21 mol% CeO2–ZrO2 before and after correction for specimen charging compared with the ELNES from the Ce M4,5-edge from 21 mol% CeO2–ZrO2. All have had the background subtracted. |
|
Figure 7
The Ce M4,5-edge XANES from 40 wt% graphite and 60 wt% of 21 mol% CeO2–ZrO2 before and after correction for specimen charging compared with the ELNES from the Ce M4,5-edge from 21 mol% CeO2–ZrO2. All have had the background subtracted. |