view article

Figure 8
Comparison of the O K-edge XANES from 40 wt% graphite and 60 wt% of 25 mol% Y2O3–ZrO2 at each stage of processing. GU-CU: graphite uncorrected, charged uncorrected; GC-CU: graphite corrected, charged uncorrected; GC-CC: graphite corrected, charged corrected. Also shown is the ELNES from 25 mol% Y2O3–ZrO2. All have had the background subtracted.