Figure 2
The In–Bi phase diagram. (Upper plot) Ambient pressure: stoichiometric compounds In2Bi, In5Bi3 and InBi. (Lower plot) High pressure, ∼10–20 GPa: phase sequence fct c/a > 1 → fct c/a < 1 → bct c/a < 1 → Cmca (see text). |
|
Figure 2
The In–Bi phase diagram. (Upper plot) Ambient pressure: stoichiometric compounds In2Bi, In5Bi3 and InBi. (Lower plot) High pressure, ∼10–20 GPa: phase sequence fct c/a > 1 → fct c/a < 1 → bct c/a < 1 → Cmca (see text). |