Figure 5
Absorption efficiency of more current scintillators used for high-resolution X-ray imaging for 5 µm-thick layers: Lu3Al5O12 (6.6 g cm−3), Gd3Ga5O12 (7.09 g cm−3), Lu3Ga5O12 (7.5 g cm−3), Lu2O3 (8.4 g cm−3), Lu2SiO5 (7.4 g cm−3), Y3Al5O12 (4.55 g cm−3) and CdWO4 (7.9 g cm−3). |