Figure 1
Temperature-dependent in situ XAS measurements at the Fe K-edge of Fe2O3@CMK-1 during reduction with hydrogen in nitrogen. |
|
Figure 1
Temperature-dependent in situ XAS measurements at the Fe K-edge of Fe2O3@CMK-1 during reduction with hydrogen in nitrogen. |