Figure 2
Scintillation intensity versus X-ray energy of the 50 min-annealed Eu-doped FCZ glass ceramic before (open squares) and after (full squares) absorption correction. The thickness of the sample was ∼480 µm. For the correction, the original data (open squares) are divided by the absorption coefficient data shown in Fig. 1 . The dashed curve shows the total mass attenuation coefficient without coherent scattering calculated from https://physics.nist.gov/PhysRefData/Xcom/html/xcom1.html
. The inset shows the Ba K-edge at 37.4 keV. |