view article

Figure 5
Visible-light absorption spectra of colloidal gold particles produced by different X-ray exposure times (30 s, 1 min, 5 min, 15 min) for a 10 ml precursor solution ([HAuCl4] = 1 mM). Note the dramatic change between 1 and 5 min exposure.