Upper panels: SAXS patterns of polyethylene, water and silver behenate collected at the SAXS station of the I711 beamline with a photon energy of 10 keV (1.2 Å). The polyethylene gives a maximum 10.4 cm−1 at 0.025 Å−1. Lower panel: SAXS pattern of colloidal polystyrene particles in water (1 wt%) as measured at the I711 beamline at MAX-lab (open squares). The average radius of the particles is 33 nm.