research papers
Energy-dispersive X-ray absorption spectroscopy at LNLS: investigation on strongly correlated metal oxides
aLaboratório Nacional de Luz Síncrotron – LNLS, CP6192, 13084-971 Campinas, SP, Brazil, bInstitut Néel, CNRS and UJF, BP 166, 38042 Grenoble, France, cComision Nacional de Energia Atómica, Centro Atomico Bariloche and Instituto Balseiro, Bariloche, Argentina, dLaboratorio Nacional de Investigacion y Servicios en Espectroscopia Optica – CEQUINOR, Universidad Nacional de La Plata, La Plata, Argentina, eInstituto de Ciencia de Materiales de Madrid, CSIC, Cantoblanco, Madrid, Spain, and fSynchrotron SOLEIL, L'Orme des Merisiers, Saint-Aubin, France
*Correspondence e-mail: helio.tolentino@grenoble.cnrs.fr
An energy-dispersive X-ray absorption spectroscopy beamline mainly dedicated to X-ray
(XMCD) and material science under extreme conditions has been implemented in a bending-magnet port at the Brazilian Synchrotron Light Laboratory. Here the beamline technical characteristics are described, including the most important aspects of the mechanics, optical elements and detection set-up. The beamline performance is then illustrated through two case studies on strongly correlated transition metal oxides: an XMCD insight into the modifications of the magnetic properties of Cr-doped manganites and the structural deformation in nickel perovskites under high applied pressure.Keywords: XAS; XMCD; high pressure.
1. Introduction
The Brazilian Synchrotron Light Laboratory (LNLS, Campinas, Brazil) runs a 1.37 GeV electron storage ring (Rodrigues et al., 1998) endowed with a 120 MeV LINAC and 500 MeV booster injector system (Lin et al., 2001) operating at a maximum current of 300 mA. The energy-dispersive X-ray absorption spectroscopy (EDXAS) beamline described here is installed in a bending-magnet port and was delivered to the users in 2005. The peculiar capability of an EDXAS spectrometer is to collect full absorption spectra through a parallel detection scheme over an extended range of photon energies without any mechanical movement (Phizackerley et al., 1983; Dartyge et al., 1986). The parallel detection, combining good spatial resolution, ability to handle the high of photons (of the order 1011 photons s−1) and fast readout times makes EDXAS specially suited to detecting very weak signals in XANES (X-ray absorption near-edge spectroscopy) and XMCD (X-ray magnetic circular dichroism) experiments (Baudelet et al., 1991; Pizzini et al., 1995), for tracking time-dependent evolution of chemical reactions (Tourillon et al., 1986) and attaining nanosecond resolution (Bonfim et al., 1998). Owing to the absence of moving parts during the acquisition, the beam in an EDXAS set-up is inherently highly stable in both energy scale and spatial position. These features, along with the intrinsic focused beam and the parallel detection, enable high-pressure studies using diamond anvil cells (Itié et al., 1989; Pascarelli et al., 2004), even when associated with XMCD experiments (Mathon et al., 2004), and the possibility of probing femtometer-scale atomic displacements (Pettifer et al., 2005).
From 2005 onwards, many experimental facilities have been developed at the LNLS EDXAS beamline; for example, a halogen-lamp-based furnace for controlled thermal treatments and study of dynamical processes (Meneses et al., 2006). This furnace made possible the observation of NiO nanoparticles undergoing a phase transformation (amorphous to nanocrystal) during annealing (Meneses et al., 2007). A reactor chamber (Bernardi et al., 2007) was used to monitor the chemical environment of Pt atoms in a catalytic reaction of PtxPd1−x nanoparticles (Bernardi et al., 2009). Both chambers are usually coupled to a for residual gas analysis. An electrochemical cell for in situ voltammetry analysis was employed to study the oxy–redoxy reaction of methanol on carbon-supported Pt–Ru nanocatalysts (Godoi et al., 2009). High-pressures studies have been reported in two different pressure domains, one up to 1.2 GPa using a B4C anvil cell (Ferreira et al., 2009) and another up to 15 GPa using a perforated diamond cell (Ramos et al., 2007). A set-up for grazing-incidence X-ray resonant magnetic scattering (Souza-Neto et al., 2006) and the use of a closed-cycle He cryostat associated with a 0.9 T permanent magnet for XMCD experiments (Azimonte et al., 2007; Stewart et al., 2007) have also been reported. Many other experiments on magnetic materials will soon become feasible with the forthcoming installation of a 6.5 T superconducting magnet. As may be noted, the LNLS EDXAS beamline covers the traditional fields of similar existing facilities around the world. Some strengths and limitations when compared with these facilities will be discussed throughout the paper.
We will give here an extensive description of the EDXAS beamline that includes the optical elements, some important aspects of the mechanics, and the detector system. Then, the beamline performance is illustrated by two studies related to main instrumental developments of the beamline: an XMCD set-up is used to study the magnetic properties of Cr-doped manganites and a diamond anvil cell is used to study the structural changes of nickel perovskites under high pressure.
2. The energy-dispersive X-ray spectrometer
The energy-dispersive X-ray spectrometer uses a bent Si crystal monochromator to provide a continuous energy variation of the Bragg-reflected photons (Fig. 1). The monochromator is bent in such a way that the incidence angle of the white synchrotron light beam changes continuously along the crystal, thus selecting a bandwidth of hundreds of eV and focusing it horizontally at the sample position. There is a correlation between the photon energy and the horizontal position at the detector. A complete X-ray is collected in a single detector's readout. Vertical focusing as well as harmonic rejection are accomplished by a bendable mirror before the Si crystal.
2.1. The energy-dispersive optics
The source-to-crystal and crystal-to-focus distances in Fig. 1 are represented by the variables p and q, respectively. The average curvature radius R is related to p and q by 1/p + 1/q = 2/(RsinθB), where θB is the average of reflection. The photon energy E depends on the θB according to E [eV] = 12398/(2d [Å] sinθB), where d is the Si spacing. The angle changes along the illuminated crystal length L, yielding a relative energy bandwidth ΔE/E = ΔθcotθB, with Δθ = L/R(1 − RsinθB/p). The full energy bandwidth is focused at the sample. The energy resolution depends essentially on the intrinsic crystal band-pass, spatial resolution of the detector and horizontal source dimension. In order to optimize energy resolution the detector is normally placed at a distance b from the sample such that b ≃ q (Tolentino et al., 1988). As can be noted, energy band-pass and resolution depend on intrinsic as well as on extrinsic parameters, like L, R and p.
The EDXAS beamline at LNLS is installed on a bending-magnetic port (Fig. 2). The horizontal and vertical dimensions (FWHM) of the source are sx = 750 µm and sy = 168 µm, respectively. The source-to-crystal distance was chosen as short as possible (p = 9.75 m) to provide a large beam horizontal acceptance by the bent crystal. This acceptance is limited to a maximum of 4.8 mrad by the detector horizontal acceptance. The crystal-to-detector distance is adjustable between 1 and 3.5 m. The 2θ arm can be adjusted to angles between 56 and 16°, providing, in principle, an energy range from 4 to 14 keV with the Si(111) crystal. A compromise between energy band-pass, energy resolution and sample position has to be found for each experimental situation. The energy band-pass and energy resolution for typical q values and at b ≃ q are presented in Figs. 3(a) and 3(b), respectively. The dotted lines in Fig. 3(a) represent the band-pass limited by the crystal size while the continuous ones give the band-pass limited by the detector window when b ≃ q. One may set the distance b smaller than q to gain band-pass with the drawback of losing energy resolution.
The lowest attainable energy depends on the sample and on its environment, especially when extreme conditions are required. Up to now, the lowest energy achieved in a real experiment is the one reported here for Cr-doped LaMnO3. The La L2 edge (5891 eV) is easily accessible owing to its high absorption However, the strong attenuation imposed by La atoms, whose L3 and L2 edges are at 5483 eV and 5891 eV, respectively, makes experiments at the Cr K edge very challenging, especially when only 5% of Cr atoms substitute for Mn atoms in the perovskite structure.
The monochromator bender mechanism developed at LNLS is detailed elsewhere (Neuenschwander & Tolentino, 2004). Such a bender is supported by four columns and assembled on top of a three-circle goniometer with the center of the crystal's front face coincident with the three-circle confusion sphere (Fig. 4). The main circle is used to set the energy, and the others are used for the preliminary alignment procedure. The vacuum vessel allows future installation of a second bender, with a different crystal reflection plane, to extend the covered energy range. All elements inside the vessel are UHV-compatible and isolated from the beamline by a 0.125 mm Be entrance window. The beam-output window is a flat 385 mm-long 10 mm-wide 0.125 mm-thick Be foil brazed on a stainless steel flange, equipped with a pneumatic shutter. A 340 l s−1 ion pump, assembled on the chamber, provides vacuum conditions without any vibration. The monochromator operates with a base pressure of 5.0 × 10−8 mbar that prevents crystal surface degradation.
The curvature radius R of the Si crystal is given by two independent torques imposed by linear actuators at each extremity. The mechanism is designed to bend a 300 mm × 20 mm rectangular crystal from 8 m to 3 m, given by a displacement of 2.3 mm of the actuator, without displacement of the central part (Neuenschwander & Tolentino, 2004). The combination of the two independent torques at each crystal extremity provides a way to significantly reduce spherical aberrations. One of the frames that transmit torque to the crystal is assembled on an elastic link enabling twist correction. A 0.25 mm eccentric twist stroke is essential for further focus optimization.
Fig. 5 presents a comparison in a situation where the aberrations are minimized with equal applied torques on both extremities (Fig. 5a) and the same situation where the two torques are optimized independently (Fig. 5b). The measurements were accomplished around the Co K edge (7709 eV) by scanning a 20 µm slit laterally through the focus position, while collecting images in the CCD-based detector. The vertical axis corresponds to the slit relative translation and the horizontal axis to the photon energy. The beam size (FWHM) at each energy is 125 µm for both situations, given by source size (750 µm) and a demagnification (q/p) of 1/6. However, one can observe that the full band-pass is spread over 350 µm when symmetric torques are applied and the focus spot is dominated by the spherical aberrations. On the other hand, when the focus is optimized, by applying asymmetric torques the aberration is reduced to less than 30 µm and the full band-pass is focused within 150 µm. The horizontal beam size that should be considered is in fact about 250 µm (full beam) when the tails are included to have more than 95% of the photons. The remaining S-shape aberration could be further reduced by a small correction in the rectangular crystal shape. This correction has not been implemented at the EDXAS beamline because the focused beam is largely limited by the bending-magnet source size, and demagnification and aberrations contribute less than 10% to the beam size. For a horizontal beam slit down to the full beam, the tails of the Gaussian-shaped beam have negligible contribution to the intensity.
Vertical focusing and harmonic rejection are provided by an 800 mm-long Rh-coated glass mirror at 6.5 m from the source (Neuenschwander & Tavares, 2001). The mirror is separated from the front-end and the monochromator by two 125 µm-thick Be windows and operates with a base pressure of 1.0 × 10−8 mbar. The bending mechanism yields at the sample a vertically focused beam (FWHM) of about 200 µm, limited by the storage ring vertical emittance and a demagnification close to 1:1. The mirror provides a cut-off energy of about 15 keV at a grazing angle of 4 mrad, the typical working angle for most experiments. At photon energies lower than 7 keV and strongly absorbing samples, the grazing angle has to be increased up to 4.5 mrad to reduce the cut-off energy to about 12 keV. A second small mirror is normally installed, between the sample and the detector, for further reducing harmonic contamination.
The bending-magnet source, front-end and et al., 2005b). In normal operation conditions, the in a spot of 250 µm × 200 µm at the sample is of the order of 1.0 × 1011 photons s−1 at 8 keV. This corresponds to the Si(111) crystal monochromator (bandwidth of 0.013%) accepting a horizontal divergence of 4 mrad and the storage ring working with 200 mA. The can be improved by a factor of two at 8 keV by pumping along the beam path. Pumping the beam path is compulsory when working at energies lower than 7 keV. For instance, at the Cr K edge (5898 eV) the is improved by one order of magnitude, from 6.0 × 1010 photons s−1 up to 4.0 × 1011 photons s−1. It must be noted that the beam path in the air is the most severe factor of attenuation and not the four 125 µm-thick Be windows, whose contribution to the attenuation is only 20% (Tolentino et al., 2005b). Such is smaller by a factor of ten when compared with a similar facility, the ODE beamline at Soleil, and by four to five orders of magnitude when compared with the undulator beamline ID24 at ESRF.
characteristics have already been discussed elsewhere (Tolentino2.2. The CCD-based detection scheme
The high ). The cryogenically cooled CCD camera system has a front-illuminated scientific grade 1 CCD of 1340 × 1300 pixels. Each pixel is 20 µm × 20 µm providing an image area of 26.8 mm × 26.0 mm. A 20 µm-thick P43 (Gd2O3S:Tb) fluorescence screen, optimized for 8 keV X-rays (Koch, 1994), receives the incoming beam at an angle of 20°. A set of lenses guides the light from the screen to the CCD detector with a demagnification factor of 1:1.75, so that the projected pixel size and useful area at the fluorescence screen are 35 µm × 35 µm and 46.9 mm × 46.5 mm, respectively. Actually, the spatial resolution measured in the energy dispersion direction is about 2.5 to 3 times larger than the projected pixel, i.e. 100 µm, owing to the penetration and blurring into the fluorescence screen. To improve spatial resolution, which turns out to be the limiting factor in the overall energy resolution, thinner fluorescence films should be considered, with the drawback of losing quantum efficiency.
is handled by a modified CCD camera that uses a phosphor screen to convert X-rays into visible light (Fig. 6The photon energy–direction correlation is transformed into an energy–position correlation along the horizontal dimension of the CCD detector. The intensity along one horizontal line of pixels gives an 5 photons of 6 keV (or, with about 275000 electrons). So, if 1.0 × 1011 photons s−1, distributed within typically 1000 horizontal by 40 vertical pixels, reach the detector, each pixel receives on average 2.5 × 106 photons s−1. The pixels at the maximum of the Gaussian distribution receive on average 5.0 × 106 photons s−1 and would saturate in about 40 ms. Typical accumulation time for frames is 20 to 1000 ms, depending on and sample attenuation. So, the intensity at each point in an frame comes from 4.0 × 106 photons at most and the statistical noise would be 5.0 × 10−4. Unfortunately, the noise level in the detector system is not coming from the counting statistics of photons; it is also dependent on charges from thermal activation, leaks and transfer processing. Beam fluctuations and instabilities along with sample inhomogeneities may also have an important impact on the noise level. The final spectrum is the average of many frames, ensuring a good signal/noise ratio is achieved.
signal. With 20° of incidence, the vertical beam (200 µm FWHM) is spread over about 18 pixels. To produce an frame, the signal is integrated along the vertical dimension over 30 to 50 pixels. Each pixel in the CCD detector is an integrator. It accumulates charges that are transferred to a processing system. A pixel saturates with about 2.0 × 102.3. The optical bench
The 2θ optical bench (Fig. 7, see also Fig. 2) is made of a steel-framed 3 m-long granite block, with two main steel rails screwed directly onto aluminium reference pads aligned on the granite block. The optical bench can bear heavy equipment and hold movable supports that are clamped to the steel rails through linear sliders. We should recall that the crystal monochromator and its internal mechanics are isolated from the vacuum chamber and supported directly in a concrete block on the floor. This makes access to the center of rotation of the monochromator difficult and imposes the design of a 2θ arm rotation based on two translation stages equipped with linear encoders, ball screws and linear bearings (Neuenschwander & Tolentino, 2004). After a proper alignment procedure, a set of equations that control each translation stage displacement is found in order to give a rotation referenced to the center of the monochromator. The rotation covers the 2θ range from 16 to 56°. The translation stages are both perpendicular to the optical bench at an angle of 36° (Fig. 2). The short stage (shown in Fig. 7) has the moving carriage equipped with a rotation platform that contains a pivoting base plate. The long stage (not seen in Fig. 7) has the moving carriage equipped with another linear stage able to move freely in the perpendicular direction. The 2θ arm is screwed onto the base plate of the short stage and placed by gravity in the center of an axial bearing at the top of the long stage. Recently, in order to receive the new 6.5 T superconducting magnet facility, the optical bench has been modified, keeping the same design but with the main rotatable arm much lower than the one shown here.
3. Case study 1: XMCD in Cr-doped LaMnO3+δ
Doped LaMnO3 perovskites have been extensively studied owing to their colossal magneto-resistance (CMR) property and its potential applications to magnetic devices (Ramirez, 1997). In Cr-doped manganites the chromium takes the Cr3+ form. This ion involves three electrons in the one-spin state of the t2g orbitals, analogous to Mn4+. For low doping concentrations, Cr3+ ions go into the Mn3+ sites, thereby changing the Mn3+ density without large distortion of the crystal cell (Morales et al., 2008). These features make the partial substitution of Mn by Cr in LaMnO3.00+δ an interesting system for studying the character of the Mn3+–Cr3+ interaction (Sun et al., 2001; Morales et al., 2005; Deisenhofer et al., 2002) and understanding the mechanism involved in CMR.
We present here a preliminary XMCD study in a series of LaMn1−xCrxO3.00+δ compounds with rigorously controlled stoichiometry. Polycrystalline powdered samples of LaMn0.75Cr0.25O3.00, LaMn0.9Cr0.1O3.04 and LaMnO3.09 were prepared by the liquid-mix method (Morales et al., 2008). X-ray powder diffraction reveals the existence of single-phase materials with orthorhombic symmetry (Pnma). With the increase of Cr content the magnetic phases change from A-type AFM order to a system with FM clusters. In sample A (LaMn0.75Cr0.25O3.00) there are no Mn4+ ions, the FM ordering temperature is 90 K and the is 1.6 μB. The holes (25%) are all introduced by Cr-doping. The two other samples contain the same hole ratio (18%). However, in sample B (LaMnO3.09) the holes are introduced only by the oxygen over-stoichiometry, then formally present as Mn4+ ions, while in sample C (LaMn0.9Cr0.1O3.04) half of them are provided by Cr-doping. The magnetic moments for samples B and C are 3.0 μB and 2.5 μB (Morales & Caneiro, 2003), with ordering temperatures of 165 K and 135 K (Morales et al., 2004), respectively. At the Mn K edge, the XMCD is due to the orbital magnetization of 4p-projected density of unoccupied states (Guo, 1998). These states are hybridized with the spin-polarized 3d Mn band, which dominates the magnetic properties of the system. Thus the XMCD amplitude reflects the Mn strength.
XMCD spectra at the Mn and Cr K edges (6539 eV and 5989 eV, respectively, in the pure elements) were collected with an average storage ring current of 250 mA. The circularly polarized light was selected 0.14 mrad (0.8 mm) above the orbital plane, with a slit aperture of 0.02 mrad (100 µm). Under such conditions the reaching the sample was reduced to about 5.0 × 1010 photons s−1 with an estimated polarization ratio of 70% (Tolentino et al., 2005a). A band-pass of 230 eV with an energy resolution of 1.5 eV was selected around the chosen edge by the Si(111) bent crystal. The beam was focused horizontally to a spot of 200 µm and collimated vertically to about 100 µm. Data were collected using the CCD detector, with the sample temperature fixed at 20 K using a closed-cycle helium cryostat. The direction of the 0.9 T applied magnetic field was inverted by 180° rotation of the permanent magnet. To avoid long-term shifts in energy scale, the sequence of collection followed the standard procedure with the magnetic field aligned parallel to the beam direction (+), then antiparallel (−), then again antiparallel (−), then finally parallel (+). The sequence is repeated starting with antiparallel, leading to the XMCD signal as the average of these eight (+−−+−++−) acquisitions. The typical acquisition time for each frame was 300 ms. Each acquisition was the result of typically 50 accumulations, or about 15 s. So, a total of 50 × 106 photons were accumulated at each acquisition, giving a statistical fluctuation of 1.4 × 10−4. However, the noise in this experiment was not limited by the Beam fluctuations and sample vibrations, induced by the rotation of the magnet, associated with sample inhomogeneities, were probably the main source of noise. Many successive acquisitions, typically 100 to 500, were added up in order to obtain a noise-to-signal ratio of the order of 10−4.
Since the Cr K and La L2 edges are only 100 eV apart (5989 eV and 5891 eV, respectively), the XANES features of the former are superimposed on the (extended X-ray absorption fine structure) oscillations of the latter. Although La is a nominally diamagnetic ion, a strong XMCD signal at the La L2 edge is clearly observed (Fig. 8). This signal is likely to arise from a ferromagnetic-induced moment by interactions with neighboring Mn ions. The La L2 background signal, extending over a large energy range far above the Cr K edge, is therefore not removed by performing differences among sequential spectra. The data presented in Fig. 8 correspond to the sample A, with the higher Cr content, and an accumulated acquisition time of about 5 h, giving a noise level of 1.5 × 10−4, which represents the RMS statistics of the spectrum when it is normalized to the La L2 edge. If the spectrum is normalized to the Cr K edge, whose jump is about ten times smaller, the noise level is of the order of 10−3. Within such a noise level, no Cr K-edge XMCD signal has been observed. As we will see below, the XMCD amplitude at the Mn K edge, which refers to the amplitude of the first negative feature around 6553 eV, ranges from 1.4 to 2.5 × 10−3. If Cr were coupled antiferromagnetically or ferromagnetically with Mn, one would expect a value quite close to that of Mn. We can conclude that either the Cr spins are randomly oriented and average out, or they give a contribution to the XMCD signal by less than 10−3. To be able to extract any signal smaller than that, at least one order of magnitude should be gained in the noise-to-signal ratio. In this experiment the noise was not limited by the counting statistics of photons but by a combination of source instabilities, inhomogeneities of the sample and sample holder vibrations. New dedicated measurements, with longer acquisition time, should significantly improve the noise-to-signal ratio.
The normalized XANES spectrum at the Mn K edge, its first derivative and the XMCD signal in LaMnO3.09 (sample B) are shown in Fig. 9 for a total acquisition time of 3 h. The XMCD and the XANES derivative shapes are quite different. Some of their near-edge features are almost out of phase, testifying that the XMCD is not a derivative spurious signal. The XANES first derivative can be used to estimate the beamline stability required for detecting reliable XMCD signals. In the present case, the maximum derivative at the edge position is about 2.3 × 10−4 meV−1. This means that, in the procedure of difference among successive spectra, an instability in the energy scale of 1 meV would give rise to a spurious contribution of 2.3 × 10−4 and then hinder any expected XMCD contribution of same order of magnitude. The noise level of our XMCD data is 1.0 × 10−4. Successive measurements of the same sample for several hours show a variation smaller than 10% in signal amplitude, thus attesting an energy stability of the order of 1 meV. For the sample B, the Mn K-edge XMCD amplitude is 2.5 × 10−3 (or 3.6 × 10−3, if corrected by the polarization ratio of 70%), in agreement with those found in doped manganites compounds with similar hole doping (Subias et al., 1997).
The XMCD signals of the different samples A, B and C (Fig. 9 and insert) have the same shape, already identified in doped manganites: a main signal changing from negative to positive at the edge, then a second resonance stemming from multiple scattering of magnetic nearest neighbors, and finally a further peak, observed at 43 eV above the edge, assigned to a simultaneous excitation of 1s and 3p electrons (Subias et al., 1997). We note that the XMCD amplitudes are very similar for samples B (2.5 × 10−3) and C (2.3 × 10−3), and about half in amplitude for sample A (1.4 × 10−3). The lower amplitude in sample A is easily explained considering that the of this sample (1.6 μB) is half that of sample B (3.0 μB). This is consistent with the strong domination of the 3d Mn spins on the magnetic properties of manganites. More singular is the similarity of the XMCD signals for samples B and C. While in the case of the mixed (hole plus Cr-)doped sample C the total is significantly (20%) smaller (2.5 μB) with respect to the strictly hole-doped sample B (3.0 μB), the XMCD signals for both samples are the same within the accuracy of 10%. The Mn atoms in both samples polarize the 4p states in the same manner and then carry similar magnetic moments. A lower for sample C could be related to an AFM Mn3+ and Cr3+ spin alignment. Further measurements are needed to confirm and extend this assumption.
4. Case study 2: pressure-induced metal–insulator transition in YNiO3
Distorted nickel perovskites RNiO3 (R = Y or rare-earth) exhibit a narrow thermally induced insulator–metal (IM) transition (except for La) (Lacorre et al., 1991). The transition temperature (TIM) increases when the R atomic size decreases. For the largest sizes (R = Pr, Nd, Sm) diffraction measurements show an orthorhombic structure with a unique rather symmetric Ni site (García-Muñoz et al., 1992). For the smallest sizes (R = Y, Ho–Lu) a monoclinic structure shows up below TIM. This monoclinic structure is characterized by the presence of two distinct Ni sites with different average Ni—O distances, both exhibiting a limited distortion of the NiO6 octahedra (Alonso et al., 1999). and XANES provided evidence for two Ni sites in the insulating phase even in the compound with orthorhombic structure (Piamonteze et al., 2005a; Acosta-Alejandro et al., 2008). The site with the longer Ni—O distances is less hybridized and promotes electronic localization. Charge-transfer multiplet simulations of the modifications in the Ni L-edge spectral shape for the insulating and metallic states undoubtedly confirmed this scenario (Piamonteze et al., 2005b).
The stability of the insulating charge-ordered state in YNiO3 under applied pressure was investigated by infrared spectroscopy and X-ray diffraction (García-Muñoz et al., 2004). The authors report a sudden structural modification close to 14 GPa, consistent with a monoclinic to orthorhombic transition. At this pressure an increase in electronic conductivity and a phonon screening were also observed. However, such structural modifications of long-range character could not be directly associated with the insulator–metal transition.
We report here on the evolution under pressure of the local scale environment of Ni3+ ions in YNiO3, directly studied by high-pressure at the Ni K edge (8345 eV). A fine-grained high-quality YNiO3 polycrystalline powder sample (Alonso et al., 2000) was loaded into the 125 µm-diameter hole of an iconel gasket mounted on 2.4 mm-thick diamond anvils. At 8 keV such thickness results in an attenuation of 96% of the incident beam. In order to keep a similar of the CCD detector, the normalization intensity without the sample was measured through an equivalent hole gasket and attenuated by thin glass plates. Each frame was collected in 100 ms and accumulated 250 times, giving a total acquisition time of 20 s per spectrum. Five spectra were collected at each pressure and then averaged to produce the final data. was measured with an energy resolution of about 1.5 eV, a band-pass of about 800 eV being focused to a Gaussian spot of 130 µm (FWHM). For each energy the center position was dispersed in less than 30 µm, in such a way that almost the whole energy band-pass could be collected through the gasket. Quasi-hydrostatic pressures up to 20 GPa were applied using silicone oil as pressure medium. The actual pressure was increased by steps of about 2 GPa, monitored and controlled with a precision of about 0.5 GPa, using the luminescence from ruby spheres. After each pressure measurement, the cell was carefully realigned at the optical focus. The energy calibration stability was better than 0.03 eV over the whole set of measurements.
Fig. 10 shows the Ni K-edge XANES spectra of YNiO3 at selected pressures. Two main changes are observed when increasing applied pressure: a shift of the and a subtle raise of the structures B and C above the edge; the feature A does not change. The shifts almost continuously towards higher energies. In order to properly interpret this shift, the reproducibility of the edge position was checked to be better than 30 meV. The accuracy can also be certified by the fact that feature A does not change and that after pressure release the features are rather recovered. The amplitude of the edge shift as a function of the increment of applied pressure, δE/δP, is not constant over the whole pressure range (insert Fig. 10). Up to about 13 GPa, δE varies almost linearly with the applied pressure and quotes about 60 meV GPa−1. Above that, δE/δP drops to 20 meV GPa−1 and another almost linear regime takes place. As the metal formal valence (Ni3+) does not change with the applied pressure, the edge shift (δE) results essentially from the modifications in the repulsive nearest-neighbor potential arising from the bond reduction (δR) in the coordination shell. As for other perovskite oxides, where the ratio δE/δR is roughly 10 eV Å−1 (Ramos et al., 2007), the shift may be converted directly into a compression. The compression separated in the two different linear regimes turns out to be ∼0.06 Å and 0.02 Å, respectively. It should be noted that the difference in the average distance of the two Ni sites in the monoclinic structure is ∼0.08 Å.
A subtle rise in the intensity of the structures B and C above the edge (from 8350 to 8370 eV) occurs in a narrow pressure range from 12 to 14 GPa. The sudden increase of the spectral weight of the B structure is associated with some degree of symmetrization in the average Ni site (Ramos et al., 2007). The rise of the C structure has been observed in the thermal evolution of the PrNiO3 compound across the insulator–metal transition (Acosta-Alejandro et al., 2008). It has unambiguously been associated with a change from two non-equivalent Ni sites, consistent with a local monoclinic distorted structure, to a single rather symmetric Ni site.
The for selected applied pressures, clearly show the good quality of the signal, free of spurious diffraction peaks from the diamond anvil cell, over a large extension in (kmax ≃ 12 Å−1). When the applied pressure increases, the overall structure of the oscillations remains almost unchanged but their amplitude slightly increases. Such a feature is usually associated with a decrease in the damping Debye–Waller (DW) term exp(−2k2σ2) accounting for bond length dispersion. The DW variation related to the coordination shell (inset Fig. 11) decreases almost linearly from 6 to 14 GPa. This decrease is in agreement with the reduction in the splitting of NiO distances. A complete analysis must be carried out to quantify this decrease. A similar drop was observed at the crossover of the thermally induced insulator–metal transition in NdNiO3 (Piamonteze et al., 2005a).
oscillations, given in Fig. 11All local experimental evidence coming from 3 at room temperature. In a first regime of compression, the largest distorted Ni site shrinks, while the smallest one remains almost unchanged, until symmetrization at the of ∼13 GPa. At this pressure all NiO6 octahedra then become roughly equivalent, charge delocalization takes place and the system becomes metallic at room temperature. The additional pressure effect is limited to an overall bond length reduction, with a decreased compressibility.
suggests a coherent description of the pressure-induced process leading to the insulator–metal transition in YNiO5. Summary
An overview of the EDXAS beamline implemented at the Brazilian Synchrotron Light Laboratory has been given. The choice of the optics and detection scheme has been determined by the bending-magnet source characteristics. The optics, mirror and monochromator, very close to the source, have the advantage that a large angular beam acceptance can be collected by the monochromator. Moreover, a few number of optical elements and short distances are favorable to produce a very stable beam. The large source size and a maximum demagnification of the order of 10 impose the size of the focused beam, which is typically 250 µm × 200 µm. The focus dimension is not limited by aberrations from the bent crystal but by the source size. This focus is quite large compared with facilities installed at higher-energies/lower-emittances synchrotron sources. The ODE beamline at Soleil utilizes a similar optics to produce a focus of 40 µm × 40 µm. At ID24 at ESRF, the beam size can be as small as 5 µm × 5 µm, which opens the possibility of micrometer mapping of inhomogeneous samples. A modified CCD detector that uses a fluorescence screen to convert X-rays into visible photons has been optimized to match the
conditions. Typical acquisition times from 10 ms to 500 ms are achieved in most experiments.In this paper two scientific cases related to strongly correlated metal oxides have been shown. In the first case, the magnetic properties of Cr-doped manganites were investigated by XMCD experiments. The preliminary results suggest that at least part of Cr spins are randomly distributed within the system or antiferromagnetically coupled to Mn3+spins. These results demonstrate the feasibility of experiments on diluted light metal elements in strongly absorbing compounds. In a second case study, a high-pressure diamond anvil cell was used to induce the metallic phase in YNiO3 at room temperature. The insulator–metal transition of YNiO3 under normal atmospheric conditions is 580 K and the effect of pressure is to reduce the structural distortion, decreasing the transition temperature. Much experimental evidence has been gathered providing a coherent local structural description across the IM transition. The stable 250 µm × 200 µm beam matches very well the diamond anvil cell for experiments in the pressure range up to 20 GPa.
The EDXAS beamline has proved to be a valuable tool for a variety of material science studies. The instrumentation has been used to investigate magnetic materials, via XMCD experiments, electrochemical and catalytic reactions and phase transitions under pressures up to 20 GPa, covering the fields of similar existing EDXAS facilities around the world. Owing to the LNLS storage ring characteristics, which are mostly a soft X-ray machine with a of 2.08 keV, the energy range covered by the beamline, from 4 to 14 keV, suffers from a limited Nevertheless, the fluorescence screen was optimized to gain in and this is not the most serious limitation. The quite large emittance, however, imposes a focused beam of 150 µm (FWHM), or 250 µm (full beam), and limits the highest attainable pressure using diamond anvil cells. It can also be a dramatic limitation when samples are inhomogeneous. On the other hand, the possibility of being very close to the source and the simplicity of the optics, with few optical elements, leads to a good stability over long periods.
Footnotes
‡Present address: European Synchrotron Radiation Facility, Grenoble, France.
§Present address: Advanced Photon Source, Argonne National Laboratory, Argonne, USA.
¶Present address: Swiss Light Source, Paul Scherrer Institut, Villegen PSI, Switzerland.
‡‡Present address: Condutiva Tecnologia, Campinas, SP, Brazil.
Acknowledgements
We acknowledge the LNLS technical staff. Special thanks to Milton Rocha for providing technical drawings. This work is partially supported by LNLS/ABTLuS/MCT and FAPESP (1999/12330-6). JCC, NMSN and AYR acknowledge the grants from FAPESP, CAPES and CNPq, respectively.
References
Acosta-Alejandro, M., Mustre de León, J., Medarde, M., Lacorre, P., Konder, K. & Montano, P. (2008). Phys. Rev. B, 77, 085107. Web of Science CrossRef Google Scholar
Alonso, J. A., García-Muñoz, J. L., Fernández-Díaz, M. T., Aranda, M. A. G., Martínez-Lope, M. J. & Casais, M. T. (1999). Phys. Rev. Lett. 82, 3871–3874. Web of Science CrossRef CAS Google Scholar
Alonso, J. A., Martínez-Lope, M. J., Casais, M. T., García-Muñoz, J. L. & Fernández-Díaz, M. T. (2000). Phys. Rev. B, 61, 1756–1763. Web of Science CrossRef CAS Google Scholar
Azimonte, C., Cezar, J., Granado, E., Huang, Q., Lynn, J., Campoy, J., Gopalakrishnan, J. & Ramesha, K. (2007). Phys. Rev. Lett. 98, 017204. Web of Science CrossRef PubMed Google Scholar
Baudelet, F., Dartyge, E., Fontaine, A., Brouder, C., Krill, G., Kapler, J. P. & Piecuch, M. (1991). Phys. Rev. B, 43, 5857–5866. CrossRef CAS Web of Science Google Scholar
Bernardi, F., Alves, M., Scheeren, C., Dupont, J. & Morais, J. (2007). J. Electron Spectrosc. Relat. Phenom. 156–158, 186–190. Web of Science CrossRef CAS Google Scholar
Bernardi, F., Alves, M. C. M., Traverse, A., Silva, D. O., Scheeren, C. W., Dupont, J. & Morais, J. (2009). J. Phys. Chem. C, 113, 3909–3916. Web of Science CrossRef CAS Google Scholar
Bonfim, M., Mackay, K., Pizzini, S., San Miguel, A., Tolentino, H., Giles, C., Neisius, T., Hagelstein, M., Baudelet, F., Malgrange, C. & Fontaine, A. (1998). J. Synchrotron Rad. 5, 750–752. Web of Science CrossRef IUCr Journals Google Scholar
Dartyge, E., Depautex, C., Dubuisson, J. M., Fontaine, A., Jucha, A., Leboucher, P. & Tourillon, G. (1986). Nucl. Instrum. Methods Phys. Res. A, 246, 452–460. CrossRef Web of Science Google Scholar
Deisenhofer, J., Paraskevopoulos, M., Krug von Nidda, H.-A. & Loidl, A. (2002). Phys. Rev. B, 66, 054414. Web of Science CrossRef Google Scholar
Ferreira, F. F., Correa, H. P. S., Orlando, M. T. D., Passamai, J. L., Orlando, C. G. P., Cavalcante, I. P., Garcia, F., Tamura, E., Martinez, L. G., Rossi, J. L. & de Melo, F. C. L. (2009). J. Synchrotron Rad. 16, 48–56. Web of Science CrossRef CAS IUCr Journals Google Scholar
García-Muñoz, J., Amboage, M., Hanfland, M., Alonso, J. A., Martinez-Lope, M. J. & Mortimer, R. (2004). Phys. Rev. B, 69, 094106. Google Scholar
García-Muñoz, J. L., Rodríguez-Carvajal, J., Lacorre, P. & Torrance, J. B. (1992). Phys. Rev. B, 46, 4414–4425. Google Scholar
Godoi, D. R. M., Perez, J. & Villullas, H. M. (2009). J. Phys. Chem. C, 113, 8518–8525. Web of Science CrossRef CAS Google Scholar
Guo, G. Y. (1998). Phys. Rev. B, 57, 10295–10298. Web of Science CrossRef CAS Google Scholar
Itie, J. P., Polian, A., Calas, G., Petiau, J., Fontaine, A. & Tolentino, H. (1989). Phys. Rev. Lett. 63, 4–8. CrossRef Web of Science Google Scholar
Koch, A. (1994). Nucl. Instrum. Methods Phys. Res. A, 348, 654–658. CrossRef CAS Web of Science Google Scholar
Lacorre, P., Torrance, J. B., Pannetier, J., Nazzal, A. I., Wang, P., Huang, T. & Siemens, R. (1991). J. Solid State Chem. 91, 225–237. CrossRef Web of Science Google Scholar
Lin, L., Tavares, P. F. & Tosin, G. (2001). IEEE Proc. 5, 2701. Google Scholar
Mathon, O., Baudelet, F., Itié, J.-P., Pasternak, S., Polian, A. & Pascarelli, S. (2004). J. Synchrotron Rad. 11, 423–427. Web of Science CrossRef CAS IUCr Journals Google Scholar
Meneses, C., Flores, W. & Sasaki, J. (2007). Chem. Mater. 19, 1024–1027. Web of Science CrossRef CAS Google Scholar
Meneses, C. T., Flores, W. H., Sotero, A. P., Tamura, E., Garcia, F. & Sasaki, J. M. (2006). J. Synchrotron Rad. 13, 468–470. Web of Science CrossRef CAS IUCr Journals Google Scholar
Morales, L., Allub, R., Alascio, B., Butera, A. & Caneiro, A. (2005). Phys. Rev. B, 72, 132413. Web of Science CrossRef Google Scholar
Morales, L. & Caneiro, A. (2003). J. Solid State Chem. 170, 404–410. Web of Science CrossRef CAS Google Scholar
Morales, L., Rodriguez-Carvajal, J. & Caneiro, A. (2004). J. Alloys Compd. 369, 97–100. Web of Science CrossRef CAS Google Scholar
Morales, L., Zysler, R. & Caneiro, A. (2008). J. Solid State Chem. 181, 1824–1832. Web of Science CrossRef CAS Google Scholar
Neuenschwander, R. T. & Tavares, W. S. (2001). Internal Technical Communication. Internal Technical Note, LNLS, Campinas, SP, Brazil. Google Scholar
Neuenschwander, R. T. & Tolentino, H. C. N. (2004). AIP Conf. Proc. 705, 647–650. CrossRef Google Scholar
Pascarelli, S., Mathon, O. & Aquilanti, G. (2004). J. Alloys Compd. 362, 33–40. Web of Science CrossRef CAS Google Scholar
Pettifer, R. F., Mathon, O., Pascarelli, S., Cooke, M. D. & Gibbs, M. R. J. (2005). Nature (London), 435, 78–81. Web of Science CrossRef PubMed CAS Google Scholar
Phizackerley, R. P., Rek, Z. U., Stephenson, G. B., Conradson, S. D., Hodgson, K. O., Matsushita, T. & Oyanagi, H. (1983). J. Appl. Cryst. 16, 220–232. CrossRef CAS Web of Science IUCr Journals Google Scholar
Piamonteze, C., de Groot, F. M. F., Tolentino, H. C. N., Ramos, A. Y., Massa, N. E., Alonso, J. A. & Martínez-Lope, M. J. (2005a). Phys. Rev. B, 71, 020406. Web of Science CrossRef Google Scholar
Piamonteze, C., Tolentino, H. C. N., Ramos, A. Y., Massa, N. E., Alonso, J. A., Martínez-Lope, M. J. & Casais, M. T. (2005b). Phys. Rev. B, 71, 012104. Web of Science CrossRef Google Scholar
Pizzini, S., Fontaine, A., Giogetti, C., Dartyge, E., Bobo, J.-F., Piecuch, M. & Baudelet, F. (1995). Phys. Rev. Lett. 74, 1470–1473. CrossRef PubMed CAS Web of Science Google Scholar
Ramirez, A. (1997). J. Phys. Condens. Matter, 9, 8171–8199. CrossRef CAS Web of Science Google Scholar
Ramos, A. Y., Tolentino, H. C. N., Souza-Neto, N. M., Itié, J. P., Caneiro, A. & Morales, L. (2007). Phys. Rev. B, 75, 052103. Web of Science CrossRef Google Scholar
Rodrigues, A. R. D., Craievich, A. F. & Gonçalves da Silva, C. E. T. (1998). J. Synchrotron Rad. 5, 1157–1161. Web of Science CrossRef CAS IUCr Journals Google Scholar
Souza-Neto, N. M., Ramos, A. Y., Tolentino, H. C. N., Martins, A. & Santos, A. D. (2006). Appl. Phys. Lett. 89, 111910. Web of Science CrossRef Google Scholar
Stewart, S., Figueroa, S., Sturla, M., Scorzelli, R., Garcia, F. & Requejo, F. (2007). Physica B, 389, 155–158. Web of Science CrossRef CAS Google Scholar
Subias, G., Garcia, J., Proietti, M. & Blasco, J. (1997). Phys. Rev. B, 56, 8183–8191. CrossRef CAS Web of Science Google Scholar
Sun, Y., Tong, W., Xu, X. & Zhang, Y. (2001). Phys. Rev. B, 63, 174438. Web of Science CrossRef Google Scholar
Tolentino, H. C. N., Cezar, J. C., Souza-Neto, N. M. & Ramos, A. Y. (2005a). J. Synchrotron Rad. 12, 168–176. Web of Science CrossRef CAS IUCr Journals Google Scholar
Tolentino, H. C. N., Cezar, J. C., Watanabe, N., Piamonteze, C., Souza-Neto, N. M., Tamura, E., Ramos, A. & Neueschwander, R. (2005). Phys. Scr. T115, 977–979. CrossRef CAS Google Scholar
Tolentino, H., Dartyge, E., Fontaine, A. & Tourillon, G. (1988). J. Appl. Cryst. 21, 15–22. CrossRef CAS Web of Science IUCr Journals Google Scholar
Tourillon, G., Dartyge, E., Fontaine, A. & Jucha, A. (1986). Phys. Rev. Lett. 57, 603–606. CrossRef PubMed CAS Web of Science Google Scholar
© International Union of Crystallography. Prior permission is not required to reproduce short quotations, tables and figures from this article, provided the original authors and source are cited. For more information, click here.