Figure 1
Ex situ XRD patterns of the spent (a) and fresh-g (b) catalysts. The fresh-g catalyst was sulfided in a 5% H2S/H2 stream at 673 K and 4.1 MPa. Circles: 2H-MoS2; squares: γ-Al2O3; triangles: Ni3S2. |
|