Figure 7
SXES emission intensities averaged over the ZnO plateaus from sample B (CIS) are plotted versus the ZnO layer thickness of the corresponding plateaus. The dotted lines are exponential fits to the experimental data. (a) The averaged S L2,3 emission intensity of the scan image in Fig. 6 (a). (b) The averaged combined Zn/O emission intensity of the scan image shown in Fig. 6 (b). |