Figure 2
The grid layout for strain mapping of the polycrystalline alumina specimen. X-ray readings are taken over (a) 56 locations at = 90° before the specimen is rotated to take (b) 40 readings at = 0°. The region of interest is the = 90° rotation angle for which the (c) stress maps will be plotted as shown in the example. |


journal menu![[Figure 2]](ie5044fig2.jpg)
= 90° before the specimen is rotated to take (