Figure 7
Elastic-scattering peaks from an indium foil sample measured by the energy-resolved detector with the following optical configuration: white beam, XPL, without a wire and with 0.25, 0.6, 1.0 mm wires, 20 µm pinhole, scatter sample; DMM (white beam, double multilayer monochromator, XPL, scatter sample). The intensity was normalized to the peak maximum. |