Evolution of orientation and strain with loading. (a) and (b) HETL orientation maps of the unloaded sample and after 2.4% plastic strain, respectively. (c) and (d) Schmid factor maps with respect to the macroscopic horizontal loading direction for the unloaded sample and after 2.4% plastic strain, respectively. (e) and (f) Axial stress (MPa) from XMAS refinement for the unloaded sample and after 2.4% plastic strain, respectively.