Figure 5
A unipolar PE loop measurement of the PMN–PT single crystal collected at 40 points around the electrical cycle at a frequency of 1 Hz and temperature of 298 K. A change in slope, indicating a change in crystal structure, is evident at an applied field of ∼0.7 kV mm−1. |