view article

Figure 2
M2,3-edge XAS of CoF2 (a, green), NiO (a, blue) and CuO (a, red); M2,3-edge XAS of LiNiO2 (b), NiO (c) and Ni(OH)2 (d). The vertical bars are the M2,3-edge peak positions for LiNiO2 and NiO.