Figure 1
Linear attenuation coefficient as a function of synchrotron radiation energy operated by XAS (7–20 keV) for all Bi2O3 loading (0–38 wt%) of the electrospun n-Bi2O3/PLA and m-Bi2O3/PLA nanofibre mats. |
|
Figure 1
Linear attenuation coefficient as a function of synchrotron radiation energy operated by XAS (7–20 keV) for all Bi2O3 loading (0–38 wt%) of the electrospun n-Bi2O3/PLA and m-Bi2O3/PLA nanofibre mats. |