Linear attenuation coefficient as a function of effective energy operated by various X-ray tube voltages of the mammography unit (22–49 kV) for all Bi2O3 loading (0–38 wt%) of the electrospun n-Bi2O3/PLA and m-Bi2O3/PLA nanofibre mats. |
|