Figure 4
(a) Raw 0–360° sinogram of a large sample (porous yttriz-stabilized zirconia) that is not fitting in the detector's field-of-view. (b) Paired 0–180 and 180–360° sinograms. (c) Registered sinogram using phase correlation. (d) Reconstructed image from the registered sinogram. |