Figure 9
GIXD radial scan, along the azimuth (αi = 0.2°), showing the solidification of 4 nm after exposure to SiH4; Au solidification achieved with a ΔT ≅ 50 K (intensities scaled for clarity). |
|
|
|
Figure 9
GIXD radial scan, along the azimuth (αi = 0.2°), showing the solidification of 4 nm after exposure to SiH4; Au solidification achieved with a ΔT ≅ 50 K (intensities scaled for clarity). |