Figure 3
(a) FTIR spectra of silica hybrid films exposed to increasing hard X-ray doses: not exposed (black line), exposed to 188.5 (red line), 377 (blue line), 754 (green line) and 1508 J cm−2 (pink line). (b) Integrated area % of Si—O—Si group at 1073 cm−1 (black line), —CH3 group at 1275 cm−1 (red line) and Si—OH bond at 3396 cm−1 (blue line) as a function of increasing X-ray doses. The lines are a guide for the eyes.