Figure 10
Growth of the contamination film on an initially flat surface at different values of parameter [{\eta_0}], i.e. 0.03 (a) and 0.15 (b), resulting in the probability of polymerization at a flat substrate P0 = 2.2% (a) and 10.7% (b). The ratio Pdes/Pdif = 1 is the same in both cases. The cube size is a = 0.25 nm. The same sets of random numbers {j} and {p} were used when modeling the growth of the films.