Figure 15
Dependence of the energy of the main peak of the Ti L3-edge of a TiO2 thin film from scan number, before (black squares) and after (red circles) correction with a reference sample. The inset shows the full Ti L2,3-edges XAS scan, with its main peak indicated by an arrow.