Figure 1
Grazing-incidence reflectivity curves (dots) for S1 (a), S3 (b) and S5 (c), measured when the samples were annealed at room temperature, 100, 200, 300 and 400°C, and their fitting curves (lines). |
|
Figure 1
Grazing-incidence reflectivity curves (dots) for S1 (a), S3 (b) and S5 (c), measured when the samples were annealed at room temperature, 100, 200, 300 and 400°C, and their fitting curves (lines). |