Figure 6
Photograph of a fragment of the diamond single crystal with spots A and B irradiated for 4 h by X-rays of the 12.5 kW mm−2 power density at different vacuum levels in the sample chamber: 1 × 10−8 Torr in area A, and 4 × 10−6 Torr in area B. See text for details. |