Figure 9
(a)–(b) SrTiO3 substrates fixed onto the sample holder before the two subsequent depositions of LSMO (PLD chamber) and FePc (molecular chamber). In panel (b) the position of the two masks is highlighted by a coloured squared box; (c) Fe L2,3 XAS spectra measured in the two positions drawn in (a), after molecular deposition on LSMO thin film, keeping the internal mask of 5 mm × 5 mm at a close distance with respect to the specimen.