Refined profiles of PZT-0.6 at 10 K. Experimental data: red; calculated fit: black line. Ticks below: Cm reflections – black; P4mm reflections – green; I4cm reflections – red. Results for {200}pc, {210}pc and {013}pc reflections are shown. This figure is in colour in the electronic version of this paper.