[HTML version][PDF version][Article Abstract][CIF][3d view][Structure Factors][Issue contents]  [Buy article online]

[Contents scheme]

Acta Cryst. (2006). E62, m3496-m3497  [ doi:10.1107/S1600536806049543 ]

Di-[mu]-chloro-bis({3-[(2-hydroxy-1-methyl-2-phenylethyl)iminomethyl]-2-naphtholato-[kappa]3N,O,O'}copper(II)) methanol solvate

S.-A. Li, Y.-C. Jin, T.-T. Xu, D.-Q. Wang and J. Gao

Online 30 November 2006


Key indicators

checkCIF/PLATON results

No syntax errors found




Alert level C RINTA01_ALERT_3_C The value of Rint is greater than 0.10 Rint given 0.118 PLAT020_ALERT_3_C The value of Rint is greater than 0.10 ......... 0.12 PLAT026_ALERT_3_C Ratio Observed / Unique Reflections too Low .... 48 Perc. PLAT220_ALERT_2_C Large Non-Solvent C Ueq(max)/Ueq(min) ... 2.65 Ratio PLAT232_ALERT_2_C Hirshfeld Test Diff (M-X) Cu1 - Cl2 .. 7.04 su PLAT341_ALERT_3_C Low Bond Precision on C-C bonds (x 1000) Ang ... 13 PLAT410_ALERT_2_C Short Intra H...H Contact H1 .. H10 .. 1.99 Ang. PLAT410_ALERT_2_C Short Intra H...H Contact H21 .. H30 .. 1.97 Ang.
0 ALERT level A = In general: serious problem 0 ALERT level B = Potentially serious problem 8 ALERT level C = Check and explain 0 ALERT level G = General alerts; check 0 ALERT type 1 CIF construction/syntax error, inconsistent or missing data 4 ALERT type 2 Indicator that the structure model may be wrong or deficient 4 ALERT type 3 Indicator that the structure quality may be low 0 ALERT type 4 Improvement, methodology, query or suggestion 0 ALERT type 5 Informative message, check