Figure 3
DSC and TG diagram for the second heating run of K2MoO4 synthesized with 10 wt% additional K2CO3 at 1213 K. Heating rate: 20 K min−1. Measuring conditions as for Fig. 1 . |
|
|
|
Figure 3
DSC and TG diagram for the second heating run of K2MoO4 synthesized with 10 wt% additional K2CO3 at 1213 K. Heating rate: 20 K min−1. Measuring conditions as for Fig. 1 . |