Low-angle part of the powder diffraction pattern of a magnesia screed (sample taken at the Weinhalle in Oppenweiler) at T = 295 K as a function of diffraction angle 2θ. The intensity is plotted on a logarithmic scale. The wavelength was λ = 0.64899 (2) Å. The 100% peak of chlorartinite is clearly visible.